All
concrete to be casted should be Modified with water reducing,
waterproofing admixture FAIRCRETE RMW @150ml / 50Kg of Cement. &
all construction joints to be given bond coat of FAIRBOND EP over old
concrete surface,” and all slope to be maintained towards
drainage/outlet end. (to
be under
the scope of main/civil contractor.)
WATERPROOF
BASE PREPARATION:
01-Cleaning
and washing of the surface with Wire brush /Broom.
02-Fixing
G.I.SPOUT, at the lowest end, towards outside. The tail end should be
at least 100mm away from finished wall surface.
03-Repairing/Rehabilitation
of poor concrete surface using FAIRCRETE SB (L) @ 5 %by Wt. of Cement,
followed with sealing SPOUT pipe to masonry joints with FAIRSEAL (In
case of dry surface) or with Acrylic modified putty of
CRACKSEAL (in case of wet surface).
04-Making
fillet GALTA all around by using modified Acrylic Cementitious screed
(1:2:2), by adding FAIRCRETE RMW at construction joints @ 150 ml per
50Kg bag of cement.
WATERPROOF
COATING & PROTECTION LAYER:
Applying
one coat of water based Epoxy primer of SAFECORE WB PRIMER followed
with two coats of Bituminous Epoxy coating (for protection against
water and Fertilizer ingress) of WATERGUARD CE followed with
sprinkling of Epoxy coated granular and applying spout towards the
open area.
)
|